Material Comparison

Product Info
Product Name
Brand Name
Usages
Properties
Certificates
PA66 66G25V0P DOMO CHEM GERMANY
--
--
Filler: Glass fiber reinf,25% filler by weight
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--

Plastic Datasheets

Impact resistanceTest ConditionTest MethodDOMO CHEM GERMANY/66G25V0P
Charpy Notched Impact Strength23°CISO 179/1eA5.5 kJ/m²
Suspended wall beam without notch impact strength23°CISO 180/1U30 kJ/m²
Impact strength of simply supported beam without notch23°CISO 179/1eU35 kJ/m²
Impact strength of cantilever beam gap23°CISO 180/1A5.5 kJ/m²
Mechanical propertiesTest ConditionTest MethodDOMO CHEM GERMANY/66G25V0P
Tensile modulusISO 527-2/18000 Mpa
tensile strength 断裂ISO 527-2/5110 Mpa
bending strengthISO 178170 Mpa
Flexural modulusISO 1787000 Mpa
Tensile strain断裂ISO 527-2/52.5 %
Electrical performanceTest ConditionTest MethodDOMO CHEM GERMANY/66G25V0P
Compared to the Leakage Tracking Index (CTI)解决方案 AIEC 60112 V
Volume resistivityIEC 600931.0E+15 ohms·cm
Surface ResistivityIEC 600931.0E+13 ohms
flammabilityTest ConditionTest MethodDOMO CHEM GERMANY/66G25V0P
burning rateFMVSS 302< 100 mm/min
UL flame retardant rating0.8 mmUL 94V-0
Hot filament ignition temperature1.0 到 3.0 mmIEC 60695-2-13775 °C
Burning wire flammability index1.0 到 3.0 mmIEC 60695-2-12960 °C
physical property Test ConditionTest MethodDOMO CHEM GERMANY/66G25V0P
densityISO 11831.39 g/cm³
Thermal performanceTest ConditionTest MethodDOMO CHEM GERMANY/66G25V0P
melting temperatureISO 11357-3262 °C
Heat distortion temperature0.45 MPa, 未退火,HDTISO 75-2/B240 °C
vicatISO 306/B50235 °C
Heat distortion temperature1.8 MPa, 未退火,HDTISO 75-2/A220 °C
injectionTest ConditionTest MethodDOMO CHEM GERMANY/66G25V0P
drying time2.0 to 4.0 hr
Processing (melt) temperature270 to 290 °C
drying temperature75 to 85 °C
Temperature80 to 100 °C