PA12 77G33HS1L NC010 DUPONT USA
Zytel®
Automotive sector
Aging resistance、Thermal stability
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Electrical performance | Test Condition | Test Method | DUPONT USA/77G33HS1L NC010 |
---|---|---|---|
Volume resistivity | IEC 60093 | 1E+13 E-4/C | |
UL flame retardant rating | 0.75mm | UL 94 | HB |
Compared to the Leakage Tracking Index (CTI) | 3.0mm | UL 746A | PLC 1 |
Mechanical properties | Test Condition | Test Method | DUPONT USA/77G33HS1L NC010 |
---|---|---|---|
Breaking stress | ISO 527 | 168 Mpa | |
Charpy Notched Impact Strength | -40 ℃ | ISO 179/1eA | 12 kJ/m² |
23 ℃ | ISO 179/1eA | 13 kJ/m² | |
Flexural modulus | ISO 178 | 8200 Mpa | |
Charpy Notched Impact Strength | -30℃ | ISO 179/1eA | 11 kJ/m² |
fracture strain | ISO 527 | 3 % | |
Impact strength of simply supported beam without notch | -30℃ | ISO 179/1eU | 60 kJ/m² |
23 ℃ | ISO 179/1eU | 80 kJ/m² | |
Tensile modulus | ISO 527 | 9500 Mpa |
Thermal performance | Test Condition | Test Method | DUPONT USA/77G33HS1L NC010 |
---|---|---|---|
Heat distortion temperature | 1.80MPa,HDT | ASTM D790/ISO 178 | 200 °C |
Linear coefficient of thermal expansion | Parallel | ISO 11359-1/-2 | 0.26 E-4/C |
Normal | ISO 11359-1/-2 | 0.83 E-4/C | |
melting temperature | 10°C/min | ISO 11357-1/-3 | 218 °C |
Heat distortion temperature | 0.45MPa,HDT | ASTM D790/ISO 178 | 216 °C |