Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PC G2510 PR001 UNIGEL BRAZIL
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Impact resistance | Test Condition | Test Method | UNIGEL BRAZIL/G2510 PR001 |
---|---|---|---|
Impact strength of cantilever beam gap | 3.20mm | ASTM D256 | 98 J/m |
hardness | Test Condition | Test Method | UNIGEL BRAZIL/G2510 PR001 |
---|---|---|---|
Rockwell hardness | M级 | ASTM D785 | 90 |
Electrical performance | Test Condition | Test Method | UNIGEL BRAZIL/G2510 PR001 |
---|---|---|---|
Dissipation Factor | 60Hz | ASTM D150 | 8E-04 |
dielectric constant | 60Hz | ASTM D150 | 3.10 |
Volume resistivity | ASTM D257 | 1E+16 ohms·cm | |
Dissipation Factor | 1MHz | ASTM D150 | 9E-03 |
dielectric constant | 1MHz | ASTM D150 | 2.95 |
dielectric strength | 1.60mm | ASTM D149 | 22 kV/mm |
arc resistance | ASTM D495 | 110 sec |
Mechanical properties | Test Condition | Test Method | UNIGEL BRAZIL/G2510 PR001 |
---|---|---|---|
Flexural modulus | ASTMD790 | 3920 MPa | |
elongation | 断裂 | ASTMD638 | 5.0 % |
Tensile modulus | ASTMD638 | 3900 MPa | |
tensile strength | 断裂 | ASTMD638 | 83.0 MPa |
屈服 | ASTMD638 | 88.0 MPa | |
bending strength | ASTMD790 | 120 MPa |
flammability | Test Condition | Test Method | UNIGEL BRAZIL/G2510 PR001 |
---|---|---|---|
Hot filament ignition temperature | 3.2mm | IEC 60695-2-13 | 960 °C |
physical property | Test Condition | Test Method | UNIGEL BRAZIL/G2510 PR001 |
---|---|---|---|
Shrinkage rate | MD | ASTM D955 | 0.50to0.60 % |
density | ASTMD792 | 1.27 g/cm³ | |
Water absorption rate | 23°C,24hr | ASTM D570 | 0.15 % |
Thermal performance | Test Condition | Test Method | UNIGEL BRAZIL/G2510 PR001 |
---|---|---|---|
Heat distortion temperature | 1.8MPa,未退火,HDT | ASTMD648 | 136 °C |
Linear coefficient of thermal expansion | MD | ASTM D696 | 4.5E-05 cm/cm/°C |