| thermal performance | Test Condition | Test Method | SABIC SAUDI/30YM243 |
|---|---|---|---|
| Linear coefficient of thermal expansion | 23℃-80°C | ASTM D696 | 0.000041 cm/cm/℃ |
| Hot deformation temperature | 1.8 MPa, Unannealed | ISO 75-2/A | 156 °C |
| Linear coefficient of thermal expansion | -30℃-30℃ | ASTM D696 | 0.000051 cm/cm/℃ |
| mechanical properties | Test Condition | Test Method | SABIC SAUDI/30YM243 |
| Tensile modulus | 23℃, Injection | ISO 527-2/1B | 6650 Mpa |
| 120℃, Injection | ISO 527-2/1B | 3500 Mpa | |
| tensile strength | Yield,80℃, Injection | ISO 527-2/1B | 70.0 Mpa |
| bending strength | 23℃, Injection | ISO 178 | 147 Mpa |
| Charpy Notched Impact Strength | -30℃, Injection | ISO 179/1eA | 25 kJ/m² |
| 23℃, Injection | ISO 179/1eU | 52 kJ/m² | |
| bending strength | 80℃, Injection | ISO 178 | 86.0 Mpa |
| tensile strength | Yield,23℃, Injection | ISO 527-2/1B | 110 Mpa |
| Yield,120℃, Injection | ISO 527-2/1B | 51.0 Mpa | |
| Dart impact | 23℃ | ISO 6603-2 | 58.0 J/cm |
| Charpy Notched Impact Strength | -30℃, Injection | ISO 179/1eU | 36 kJ/m² |
| Tensile strain | Break,23℃, Injection | ISO 527-2/1B | 2.3 % |
| Charpy Notched Impact Strength | 23℃, Injection | ISO 179/1eA | 19 kJ/m² |
| Tensile modulus | 80℃, Injection | ISO 527-2/1B | 4600 Mpa |
| Bending modulus | 80℃, Injection | ISO 178 | 4200 Mpa |
| 23℃, Injection | ISO 178 | 5900 Mpa |