Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

TPEE KP3339UM KOLON KOREA
KOPEL®
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
hardness | Test Condition | Test Method | KOLON KOREA/KP3339UM |
---|---|---|---|
Shore hardness | 邵氏 D | ASTM D2240 | 39 |
Mechanical properties | Test Condition | Test Method | KOLON KOREA/KP3339UM |
---|---|---|---|
tensile strength | 断裂, 3.20 mm | ASTM D638 | 25.0 Mpa |
elongation | 断裂, 3.20 mm | ASTM D638 | 860 % |
bending strength | 3.20 mm | ASTM D790 | 4.00 Mpa |
Flexural modulus | 3.20 mm | ASTM D790 | 49.0 Mpa |
flammability | Test Condition | Test Method | KOLON KOREA/KP3339UM |
---|---|---|---|
UL flame retardant rating | 0.8 mm | UL 94 | HB |
physical property | Test Condition | Test Method | KOLON KOREA/KP3339UM |
---|---|---|---|
Water absorption rate | 24 hr, 23°C | ASTM D570 | 0.70 % |
melt mass-flow rate | 230°C/2.16 kg | ASTM D1238 | 12 g/10 min |
Shrinkage rate | Flow | ASTM D955 | 1.1 % |
Thermal performance | Test Condition | Test Method | KOLON KOREA/KP3339UM |
---|---|---|---|
vicat | ASTM D15253 | 138 °C | |
melting temperature | ASTM D3418 | 195 °C |
injection | Test Condition | Test Method | KOLON KOREA/KP3339UM |
---|---|---|---|
drying time | 3.0 to 8.0 hr | ||
Suggested maximum moisture content | < 0.10 % | ||
Temperature in the middle of the barrel | 200 to 220 °C | ||
Temperature at the rear of the barrel | 180 to 190 °C | ||
drying temperature | 100 to 110 °C | ||
Temperature at the front of the material cylinder | 210 to 220 °C | ||
Temperature | 20 to 40 °C | ||
Spray nozzle temperature | 210 to 220 °C |