Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PPS 6165A4 JAPAN POLYPLASTIC
DURAFIDE®
Fiber grade
Glass fiber reinforced,Flame retardant,wear resistant
UL
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
| Supplementary Information | Test Condition | Test Method | JAPAN POLYPLASTIC/6165A4 |
|---|---|---|---|
| ColourNumber | HF2000/HD9050/HD9100 |
| hardness | Test Condition | Test Method | JAPAN POLYPLASTIC/6165A4 |
|---|---|---|---|
| Rockwell hardness | M-Scale | ISO 2039-2 | 105 |
| thermal performance | Test Condition | Test Method | JAPAN POLYPLASTIC/6165A4 |
|---|---|---|---|
| Hot deformation temperature | 1.8MPa,Unannealed | ISO 75-2/A | 270 °C |
| Linear coefficient of thermal expansion | TD | Internal Method | 3E-05 cm/cm/°C |
| MD | Internal Method | 1E-05 cm/cm/°C |
| mechanical properties | Test Condition | Test Method | JAPAN POLYPLASTIC/6165A4 |
|---|---|---|---|
| Bending modulus | ISO 178 | 18300 Mpa | |
| bending strength | ISO 178 | 190 Mpa | |
| Tensile strain | Break | ISO 527-2 | 1.1 % |
| tensile strength | ISO 527-2 | 130 Mpa |
| Electrical performance | Test Condition | Test Method | JAPAN POLYPLASTIC/6165A4 |
|---|---|---|---|
| Compared to the anti leakage trace index | IEC 60112 | PLC 3 | |
| Dielectric strength | 3.00mm | IEC 60243-1 | 14 KV/mm |
| Dissipation factor | 1MHz | IEC 60250 | 2E-03 |
| 耐电弧性 | IEC 60250 | 162 sec | |
| 1kHz | IEC 60250 | 2E-03 | |
| Relative permittivity | 1kHz | IEC 60250 | 5.80 |
| 1MHz | IEC 60250 | 5.80 | |
| Volume resistivity | IEC 60093 | 8E+15 ohms·cm |
| Physical properties | Test Condition | Test Method | JAPAN POLYPLASTIC/6165A4 |
|---|---|---|---|
| Melt viscosity | 310°C,1000sec^-1 | ISO 11443 | 400000 mPa·s |
| Water absorption rate | 23°C,24hr | ISO 62 | 0.010 % |
| flammability | Test Condition | Test Method | JAPAN POLYPLASTIC/6165A4 |
|---|---|---|---|
| UL flame retardant rating | UL 94 | V-0 |