Material Comparison

Product Info
Product Name
Brand Name
Usages
Properties
Certificates
TPV 101-35 SHANGHAI LINGEN
--
Wire and cable applicatio、packing、pipeline、currency
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--

Plastic Datasheets

hardnessTest ConditionTest MethodSHANGHAI LINGEN/101-35
Shore hardness邵氏A,15秒ASTM D224035
elastomerTest ConditionTest MethodSHANGHAI LINGEN/101-35
tensile strength 100%应变ASTM D4121.10 Mpa
elongation断裂ASTM D412300 %
compression set70°C,22hrASTM D39522 %
120°C,22hrASTM D39531 %
tensile strength 屈服ASTM D4123.50 Mpa
Stretch permanent deformationASTM D4124 %
tear strengthASTM D62411.0 kN/m
compression set23°C,22hrASTM D39512 %
agingTest ConditionTest MethodSHANGHAI LINGEN/101-35
Change rate of tensile strength in air150°C,168hr6.0 %
Change rate of ultimate elongation in air150°C,168hr3.0 %
Thermal performanceTest ConditionTest MethodSHANGHAI LINGEN/101-35
brittle temperatureASTM D746-60.0 °C

Contact Us

Get App

Top