Material Comparison
Add Comparison Model
Select Products for Comparison (1/4)
Highlight Differences
Hide Same
Product Name / Manufacturer / Model
Grade
Reference Price
| optical performance | Test Condition | Test Method | Korea Daelim Basell/HP522H |
|---|---|---|---|
| turbidity | 50.0μm | Internal Method | 0.30 % |
| gloss | 45° | Internal Method | 91 |
| mechanical properties | Test Condition | Test Method | Korea Daelim Basell/HP522H |
| tensile strength | Yield | ISO 527-2/50 | 34.0 Mpa |
| Tensile strain | Break | ISO 527-2/50 | >500 % |
| Friction coefficient | Dynamic | ASTM D1894 | 0.50 |
| Bending modulus | 23°C | ISO 178 | 1450 Mpa |
| Tensile strain | Yield | ISO 527-2/50 | 12 % |
| tensile strength | Break,23°C | ISO 527-2/50 | 23.0 Mpa |
| film | Test Condition | Test Method | Korea Daelim Basell/HP522H |
| Tensile modulus | 20μm,Tangent | Internal Method | 2900 Mpa |
| elongation | Break,20μm,MD | ASTM D882 | 90 % |
| tensile strength | Break,20μm,MD | ASTM D882 | 250 Mpa |
| thermal performance | Test Condition | Test Method | Korea Daelim Basell/HP522H |
| Hot deformation temperature | 0.45MPa,Unannealed | ISO 75-2/B | 93.0 °C |
| Vicat softening temperature | ISO 306/A50 | 155 °C | |
| Physical properties | Test Condition | Test Method | Korea Daelim Basell/HP522H |
| melt mass-flow rate | 230°C/2.16kg | ISO 1133 | 2.0 g/10min |
| hardness | Test Condition | Test Method | Korea Daelim Basell/HP522H |
| Shore hardness | ShoreD | ISO 868 | 71 |