HDPE BPD4045 PEMSB MALAYSIA
--
Wire and cable、Insulation material、Insulated overhead cable
Resistance to stress crac、Good resistance to enviro、Wear and thermal deformat
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Other performance | Test Condition | Test Method | PEMSB MALAYSIA/BPD4045 |
---|---|---|---|
oxidation induction time | 210℃ | ISO TR10837 | >20 min |
Basic performance | Test Condition | Test Method | PEMSB MALAYSIA/BPD4045 |
---|---|---|---|
Carbon black content | % | IEC 811-4-1 2.5 | |
density | ISO 1183 | 952 Kg/m | |
melt mass-flow rate | 190℃/2.16kg | ISO 1133: Condition 4 | 0.2 g/10min |
190℃/5.0kg | ISO 1133: Condition 18 | 0.85 g/10min | |
density | 退火 | ISO 1872/1 | 941 Kg/m |
Mechanical properties | Test Condition | Test Method | PEMSB MALAYSIA/BPD4045 |
---|---|---|---|
elongation | 断裂 | % | IEC 811-1-1 >600 |
hardness | ISO 868 (1sec) | 62 | |
tensile yield stress | MPa | IEC 811-1-1 23 | |
Flexural modulus | ISO 178 | 850 MPa |
Electrical performance | Test Condition | Test Method | PEMSB MALAYSIA/BPD4045 |
---|---|---|---|
dielectric constant | 1 MHz | IEC 250 2.6 | |
loss factor | 1 MHz | IEC 250 <0.001 | |
Volume resistivity | Ω.cm | IEC 93 | |
Dielectric Strength | kV/mm | IEC 243 |
Thermal performance | Test Condition | Test Method | PEMSB MALAYSIA/BPD4045 |
---|---|---|---|
Linear thermal expansion | ASTM D-696(20-60℃) | 1.5×10 ℃ | |
brittle temperature | ASTM D-746 | <-100 ℃ | |
thermal conductivity | BS 874(at 23℃) |