Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PA66 A3 1 S3 AKRO-PLASTIC GERMANY
AKROMID®
Industrial applications、Automotive sector、Electric、Electronic application fi、Fasteners、Laptop case、Application in the automo
enhance、Thermal stability
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Impact resistance | Test Condition | Test Method | AKRO-PLASTIC GERMANY/A3 1 S3 |
---|---|---|---|
Impact strength of simply supported beam without notch | 23°C | ISO 179/1eU | NoBreak |
Mechanical properties | Test Condition | Test Method | AKRO-PLASTIC GERMANY/A3 1 S3 |
---|---|---|---|
Tensile modulus | ISO 527-2/1 | 2500 Mpa | |
tensile strength | 屈服 | ISO 527-2/50 | 67.0 Mpa |
Tensile strain | 断裂 | ISO 527-2/50 | 30 % |
屈服 | ISO 527-2/50 | 4.3 % |
flammability | Test Condition | Test Method | AKRO-PLASTIC GERMANY/A3 1 S3 |
---|---|---|---|
burning rate | 1.00mm | FMVSS302 | <100 mm/min |
UL flame retardant rating | 1.6mm | UL 94 | HB |
physical property | Test Condition | Test Method | AKRO-PLASTIC GERMANY/A3 1 S3 |
---|---|---|---|
moisture absorption | 70°C,62%RH | ISO 1110 | 2.5 % |
Melt volume flow rate | 275°C/5.0kg | ISO 1133 | 55.0 cm3/10min |
Thermal performance | Test Condition | Test Method | AKRO-PLASTIC GERMANY/A3 1 S3 |
---|---|---|---|
Heat distortion temperature | 0.45MPa,未退火,HDT | ISO 75-2/B | 194 °C |
melting temperature | DIN EN11357-1 | 260 °C | |
Heat distortion temperature | 1.8MPa,未退火,HDT | ISO 75-2/A | 60.0 °C |