Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PET AV2 370/B DSM HOLAND
Arnite®
Electronic and electrical components,Electrical applications,Industrial components
Glass fiber reinforced,Antichemical,Dimensional stability
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
| Other performance | Test Condition | Test Method | DSM HOLAND/AV2 370/B |
|---|---|---|---|
| UL flame retardant rating | 1.60 mm | IEC 60695-11-10, -20 | HB |
| 0.780 mm | IEC 60695-11-10, -20 | HB |
| Basic Performance | Test Condition | Test Method | DSM HOLAND/AV2 370/B |
|---|---|---|---|
| density | ISO 1183 | 1.52 g/cm³ | |
| Water absorption rate | Equilibrium, 23°C, 50% RH | ISO 62 | 0.25 % |
| Saturation, 23°C | ISO 62 | 0.50 % |
| thermal performance | Test Condition | Test Method | DSM HOLAND/AV2 370/B |
|---|---|---|---|
| Hot deformation temperature | 1.8 MPa,Unannealed | ISO 75-2/A | 225 °C |
| Linear coefficient of thermal expansion | Flow | ISO 11359-2 | 0.000030 cm/cm/°C |
| Transverse | ISO 11359-2 | 0.000070 cm/cm/°C | |
| Melting temperature | ISO 11357-3 | 255 °C |
| mechanical properties | Test Condition | Test Method | DSM HOLAND/AV2 370/B |
|---|---|---|---|
| Impact strength of simply supported beam without notch | 23°C | ISO 179/1eA | 9.0 kJ/m² |
| Tensile modulus | ISO 527-2 | 5500 MPa | |
| Tensile strain | Break | ISO 527-2 | 2.5 % |
| tensile strength | Break | ISO 527-2 | 150 MPa |
| Electrical performance | Test Condition | Test Method | DSM HOLAND/AV2 370/B |
|---|---|---|---|
| Surface resistivity | IEC 60093 | ohms | |
| Volume resistivity | IEC 60093 | ohm·cm | |
| IEC 60093 | ohm·m |