Product Name / Manufacturer / Model
Grade
Reference Price
| mechanical properties | Test Condition | Test Method | EXXONMOBIL SAUDI/5032E1 |
|---|---|---|---|
| Tensile modulus | ISO 527-2/1A/1 | 1440 Mpa | |
| Bending modulus | ISO 178 | 1430 Mpa | |
| tensile strength | Yield | ISO 527-2/1A/50 | 33.0 Mpa |
| Tensile strain | Yield | ISO 527-2/1A/50 | 9.0 % |
| hardness | Test Condition | Test Method | EXXONMOBIL SAUDI/5032E1 |
| Shore hardness | ShoreD,15Sec | ISO 868 | 70 |
| thermal performance | Test Condition | Test Method | EXXONMOBIL SAUDI/5032E1 |
| Hot deformation temperature | 0.45MPa,Unannealed | ISO 75-2/B | 86.0 °C |
| Melting temperature | ASTM D3418 | 160 °C | |
| Physical properties | Test Condition | Test Method | EXXONMOBIL SAUDI/5032E1 |
| melt mass-flow rate | 230°C/2.16kg | ISO 1133 | 3.0 g/10min |