| Filling analysis | Test Condition | Test Method | TORAY JAPAN/CM1041 |
|---|---|---|---|
| Melt viscosity | 290°C | 770 Pa·s | |
| 270°C | 1110 Pa·s | ||
| 250°C | 1780 Pa·s | ||
| Physical properties | Test Condition | Test Method | TORAY JAPAN/CM1041 |
| density | 23°C | ISO 1183 | 1.13 g/cm³ |
| Water absorption rate | 23℃, 24 hr | ISO 62 | 1.8 % |
| density | ISO 1183 | 1.13 g/cm³ | |
| Water absorption rate | 23°C,24hr | ISO 62 | 1.8 % |
| impact performance | Test Condition | Test Method | TORAY JAPAN/CM1041 |
| Charpy Notched Impact Strength | 23°C | ISO 179 | 5.5 kJ/m² |
| mechanical properties | Test Condition | Test Method | TORAY JAPAN/CM1041 |
| Bending modulus | 23°C | ISO 178 | 2500 Mpa |
| tensile strength | 23°C | ISO 527-2 | 75.0 Mpa |
| bending strength | 23°C | ISO 178 | 100 Mpa |
| 23℃ | ISO 178 | 100 Mpa | |
| Bending modulus | 23℃ | ISO 178 | 2500 Mpa |
| Charpy Notched Impact Strength | 23℃ | ISO 179 | 5.5 kJ/m² |
| Tensile strain | Break,23°C | ISO 527-2 | 50 % |
| Break, 23℃ | ISO 527-2 | > 50 % | |
| tensile strength | Yield, 23℃ | ISO 527-2 | 75.0 Mpa |
| thermal performance | Test Condition | Test Method | TORAY JAPAN/CM1041 |
| Melting temperature | DSC | 225 °C |