| mechanical properties | Test Condition | Test Method | SABIC INNOVATIVE US/HU2200-1H1000 |
|---|---|---|---|
| elongation | Break | ASTM D638 | 4.0 % |
| bending strength | ISO 178 | 228 Mpa | |
| Tensile strain | Break | ISO 527-2/5 | 4.0 % |
| Bending modulus | 50.0mmSpan | ASTM D790 | 6850 Mpa |
| Tensile modulus | ISO 527-2/1 | 6890 Mpa | |
| ASTM D638 | 6890 Mpa | ||
| tensile strength | Break | ISO 527-2/5 | 131 Mpa |
| bending strength | Yield,50.0mmSpan | ASTM D790 | 225 Mpa |
| tensile strength | Break | ASTM D638 | 131 Mpa |
| Yield | ASTM D638 | 131 Mpa | |
| Yield | ISO 527-2/5 | 131 Mpa | |
| Bending modulus | ISO 178 | 6890 Mpa | |
| elongation | Yield | ASTM D638 | 4.0 % |
| Tensile strain | Yield | ISO 527-2/5 | 4.0 % |
| thermal performance | Test Condition | Test Method | SABIC INNOVATIVE US/HU2200-1H1000 |
| Hot deformation temperature | 1.8MPa,Unannealed,3.20mm | ASTM D648 | 208 °C |
| Vicat softening temperature | -- | ISO 306/B50 | 212 °C |
| Linear coefficient of thermal expansion | MD:23to150°C | ISO 11359-2 | 2.5E-05 cm/cm/°C |
| TD:23to150°C | ISO 11359-2 | 5E-05 cm/cm/°C | |
| Hot deformation temperature | 1.8MPa,Unannealed,100mmSpan | ISO 75-2/Ae | 205 °C |
| Vicat softening temperature | ASTM D152510 | 220 °C | |
| Linear coefficient of thermal expansion | MD:-20to150°C | ASTME831 | 2.5E-05 cm/cm/°C |
| Vicat softening temperature | -- | ISO 306/B120 | 218 °C |
| Linear coefficient of thermal expansion | TD:-40to150°C | ASTME831 | 5E-05 cm/cm/°C |
| impact performance | Test Condition | Test Method | SABIC INNOVATIVE US/HU2200-1H1000 |
| Impact strength of cantilever beam gap | 23°C | ISO 180/1A | 64 kJ/m² |
| Charpy Notched Impact Strength | 23°C | ISO 179/1eA | 65 kJ/m² |
| Dart impact | 23°C,TotalEnergy | ASTM D3763 | 8.00 J |
| Impact strength of cantilever beam gap | -30°C | ISO 180/1A | 70 kJ/m² |
| Physical properties | Test Condition | Test Method | SABIC INNOVATIVE US/HU2200-1H1000 |
| melt mass-flow rate | 337°C/6.6kg | ASTM D1238 | 6.0 g/10min |
| Water absorption rate | Equilibrium,23°C,50%RH | ISO 62 | 0.55 % |
| Melt Volume Flow Rate (MVR) | 360°C/5.0kg | ISO 1133 | 7.00 cm3/10min |
| Shrinkage rate | MD:3.20mm | Internal Method | 0.30-0.50 % |
| Water absorption rate | Saturation,23°C | ISO 62 | 1.0 % |