Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

Rubber Techsil® IS808 Techsil Limited
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
hardness | Test Condition | Test Method | Techsil Limited/Techsil® IS808 |
---|---|---|---|
IRHD hardness | BS903 | 39 |
Supplementary Information | Test Condition | Test Method | Techsil Limited/Techsil® IS808 |
---|---|---|---|
VolumetricExpansion | 8.8E-04 cm/cm/°C |
Electrical performance | Test Condition | Test Method | Techsil Limited/Techsil® IS808 |
---|---|---|---|
Volume resistivity | ASTM D257 | 4.7E+14 ohms·cm | |
Surface Resistivity | ASTM D257 | 7.8E+15 ohms | |
Dissipation Factor | 1MHz | ASTM D150 | 1.2E-03 |
dielectric constant | 1MHz | ASTM D150 | 3.20 |
Uncured Properties | Test Condition | Test Method | Techsil Limited/Techsil® IS808 |
---|---|---|---|
Curing Time | 23°C | 7.0 hr | |
surface drying time | 23°C,65%RH | 4.0 min |
Cured Properties | Test Condition | Test Method | Techsil Limited/Techsil® IS808 |
---|---|---|---|
peelstrength | 14.2 N/mm | ||
compression set | 45 % | ||
tensile strength | BS903 | 2.32 MPa | |
elongation | 断裂 | BS903 | 280 % |
Tensile modulus | -- | 0.650 MPa | |
tear strength | BS903 | 5.50 kN/m | |
Shrinkage rate | <1.0 % | ||
Tensile modulus | --3 | BS903 | 0.910 MPa |
physical property | Test Condition | Test Method | Techsil Limited/Techsil® IS808 |
---|---|---|---|
density | BS903 | 1.05 g/cm³ |
Thermal performance | Test Condition | Test Method | Techsil Limited/Techsil® IS808 |
---|---|---|---|
thermal conductivity | 0.20 W/m/K | ||
Usage temperature | -60-250 °C | ||
Linear coefficient of thermal expansion | MD | 2.9E-04 cm/cm/°C |