PEEK Pyramid™ PEEK KD2000-G01 Polymics, Ltd.
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--

Plastic Datasheets

Impact resistanceTest ConditionTest MethodPolymics, Ltd./Pyramid™ PEEK KD2000-G01
Impact strength of cantilever beam gap3.18mmASTM D25691 J/m
Suspended wall beam without notch impact strengthASTM D256无断裂
hardnessTest ConditionTest MethodPolymics, Ltd./Pyramid™ PEEK KD2000-G01
Rockwell hardnessM级ASTM D785102
Mechanical propertiesTest ConditionTest MethodPolymics, Ltd./Pyramid™ PEEK KD2000-G01
elongation断裂ASTM D638>60 %
bending strength屈服ASTM D790172 MPa
compressive strengthASTM D695124 MPa
Flexural modulusASTM D7904000 MPa
Tensile modulusASTM D6383500 MPa
tensile strength 断裂ASTM D63897.0 MPa
Electrical performanceTest ConditionTest MethodPolymics, Ltd./Pyramid™ PEEK KD2000-G01
Volume resistivityASTM D2571E+16 ohms·cm
Dissipation FactorASTM D1504E-03
dielectric strengthASTM D14918 kV/mm
Surface ResistivityASTM D2572E+16 ohms
dielectric constantASTM D1503.30
flammabilityTest ConditionTest MethodPolymics, Ltd./Pyramid™ PEEK KD2000-G01
UL flame retardant ratingUL 94V-0
physical property Test ConditionTest MethodPolymics, Ltd./Pyramid™ PEEK KD2000-G01
Crystallinity<35 %
Shrinkage rateMDASTM D9551.2 %
Water absorption rate23°C,24hrASTM D570<0.20 %
densityASTM D7921.30 g/cm³
melt mass-flow rateASTM D123820 g/10min
Thermal performanceTest ConditionTest MethodPolymics, Ltd./Pyramid™ PEEK KD2000-G01
Heat distortion temperature1.8MPa,未退火,HDTASTM D648160 °C
thermal conductivityASTMC1770.25 W/m/K
Linear coefficient of thermal expansionMDASTM D6965.9E-05 cm/cm/°C
Glass Transition TemperatureASTM D3418143 °C
melting temperatureDSC340 °C