| hardness | Test Condition | Test Method | ASAHI JAPAN/H1062 |
|---|---|---|---|
| Shore hardness | ShoreA | ISO 7619 | 67 |
| Supplementary Information | Test Condition | Test Method | ASAHI JAPAN/H1062 |
|---|---|---|---|
| Styrene/rubber ratio | Internal Method | 18/82 |
| Physical properties | Test Condition | Test Method | ASAHI JAPAN/H1062 |
|---|---|---|---|
| melt mass-flow rate | 230°C/2.16kg | ISO 1133 | 4.5 g/10min |
| elastomer | Test Condition | Test Method | ASAHI JAPAN/H1062 |
|---|---|---|---|
| elongation | Break | ISO 37 | 670 % |
| tensile strength | 300%Strain | ISO 37 | 4.30 Mpa |
| Break | ISO 37 | 15.0 Mpa |