PA11/TPE 55R53 SP 01 ARKEMA USA
Pebax®Rnew®
Electric wire,Profile
UV resistance,Thermal stability
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Impact resistance | Test Condition | Test Method | ARKEMA USA/55R53 SP 01 |
---|---|---|---|
Impact strength of simply supported beam without notch | -30°C | ISO 179/1eU | 无断裂 |
23°C | ISO 179/1eU | 无断裂 |
hardness | Test Condition | Test Method | ARKEMA USA/55R53 SP 01 |
---|---|---|---|
Shore hardness | 邵氏 D, 15 秒 | ISO 7619-1 | 51 |
Mechanical properties | Test Condition | Test Method | ARKEMA USA/55R53 SP 01 |
---|---|---|---|
Tensile modulus | ISO 527-2 | -- Mpa | |
Tensile strain | 断裂 | ISO 527-2 | > 300 % |
tensile strength | 断裂 | ISO 527-2 | 45.0 Mpa |
50% 应变 | ISO 527-2 | -- Mpa |
squeeze out | Test Condition | Test Method | ARKEMA USA/55R53 SP 01 |
---|---|---|---|
drying temperature | 65 to 75 °C | ||
Melt Temperature | 200 to 270 °C | ||
drying time | 4.0 to 8.0 hr |
physical property | Test Condition | Test Method | ARKEMA USA/55R53 SP 01 |
---|---|---|---|
Water absorption rate | 平衡, 23°C, 50% RH | ISO 62 | 0.70 % |
Shrinkage rate | 流量 | ISO 294-4 | 1.0 % |
Water absorption rate | 饱和, 23°C | ISO 62 | 1.5 % |
Shrinkage rate | 横向流量 | ISO 294-4 | 1.0 % |
Thermal performance | Test Condition | Test Method | ARKEMA USA/55R53 SP 01 |
---|---|---|---|
melting temperature | ISO 11357-3 | 167 °C | |
vicat | ISO 306/B50 | 156 °C | |
melting temperature | Renewable Carbon Conent | CSA LISTED | 62 to 66 % |
injection | Test Condition | Test Method | ARKEMA USA/55R53 SP 01 |
---|---|---|---|
drying time | 4.0 to 8.0 hr | ||
Processing (melt) temperature | 210 to 230 °C | ||
drying temperature | 65 to 75 °C | ||
Temperature | 25 to 60 °C |