Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PA6 LCA® N6-33GF UniPlas, Inc.
--
--
Filler, glass fiber reinforced material, 33%, filler by weight
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Impact resistance | Test Condition | Test Method | UniPlas, Inc./LCA® N6-33GF |
---|---|---|---|
Impact strength of cantilever beam gap | ASTM D256 | 64 J/m |
Mechanical properties | Test Condition | Test Method | UniPlas, Inc./LCA® N6-33GF |
---|---|---|---|
elongation | 断裂 | ASTM D638 | 2.5 % |
bending strength | 屈服 | ASTM D790 | 214 MPa |
tensile strength | 断裂 | ASTM D638 | 128 MPa |
Flexural modulus | ASTM D790 | 8270 MPa | |
tensile strength | 屈服 | ASTM D638 | 131 MPa |
physical property | Test Condition | Test Method | UniPlas, Inc./LCA® N6-33GF |
---|---|---|---|
ash content | ASTM D5630 | 33 % | |
density | ASTM D792 | 1.39 g/cm³ |
Thermal performance | Test Condition | Test Method | UniPlas, Inc./LCA® N6-33GF |
---|---|---|---|
melting temperature | ASTM D789 | 215 °C |