| hardness | Test Condition | Test Method | OTSUKAC JAPAN/NT36 |
|---|---|---|---|
| Rockwell hardness | M-Scale | ASTM D785 | 108 |
| thermal performance | Test Condition | Test Method | OTSUKAC JAPAN/NT36 |
|---|---|---|---|
| Heat Distortion | ASTM D648 | 210 °C | |
| Linear coefficient of thermal expansion | Flow | ASTM D696 | 2.0E-5 cm/cm/°C |
| mechanical properties | Test Condition | Test Method | OTSUKAC JAPAN/NT36 |
|---|---|---|---|
| Bending modulus | ASTM D790 | 11900 Mpa | |
| bending strength | ASTM D790 | 248 Mpa | |
| elongation | Break | ASTM D638 | 3.0 % |
| Friction coefficient | 与钢 - 动态 | 0.53 | |
| tensile strength | ASTM D638 | 159 Mpa | |
| Wear amount | of counterpart 3 | 0.00 10^-3 mm³/N·km | |
| --2 | 73.5 10^-3 mm³/N·km |
| Physical properties | Test Condition | Test Method | OTSUKAC JAPAN/NT36 |
|---|---|---|---|
| Shrinkage rate | Flow | 0.40 % | |
| Across FlowFlow | 0.90 % | ||
| Water absorption rate | Equilibrium | ASTM D570 | 0.20 % |
| injection | Test Condition | Test Method | OTSUKAC JAPAN/NT36 |
|---|---|---|---|
| Injection pressure | 40.0 to 60.0 Mpa | ||
| Mold temperature | 120 to 150 °C | ||
| Processing (melt) temperature | 260 to 280 °C |