Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PA66 A3 GF 30 AKRO-PLASTIC GERMANY
AKROMID®
Industrial applications,Automotive sector,Engineering accessories,Application in the automotive field
enhance,Thermal stability,Filler: Glass fiber reinf,30%,Filler by weight
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Supplementary Information | Test Condition | Test Method | AKRO-PLASTIC GERMANY/A3 GF 30 |
---|---|---|---|
ReinforcementContent | ISO 1172 | 30 % |
thermal performance | Test Condition | Test Method | AKRO-PLASTIC GERMANY/A3 GF 30 |
---|---|---|---|
Hot deformation temperature | 8.0MPa,Unannealed | ISO 75-2/C | 210 °C |
1.8MPa,Unannealed | ISO 75-2/A | 255 °C | |
Linear coefficient of thermal expansion | TD:23to80°C | ISO 11359-2 | 9.5E-05 cm/cm/°C |
MD:23to80°C | ISO 11359-2 | 1.9E-05 cm/cm/°C | |
Melting temperature | DIN EN11357-1 | 262 °C |
mechanical properties | Test Condition | Test Method | AKRO-PLASTIC GERMANY/A3 GF 30 |
---|---|---|---|
Bending modulus | ISO 178 | 8500 Mpa | |
bending strength | ISO 178 | 280 Mpa | |
Tensile modulus | ISO 527-2/1 | 9500 Mpa | |
Tensile strain | Break | ISO 527-2/5 | 3.5 % |
tensile strength | Break | ISO 527-2/5 | 190 Mpa |
Physical properties | Test Condition | Test Method | AKRO-PLASTIC GERMANY/A3 GF 30 |
---|---|---|---|
Hygroscopicity | 70°C,62%RH | ISO 1110 | 1.9to2.1 % |
Shrinkage rate | MD | ISO 294-4 | 0.20 % |
TD | ISO 294-4 | 1.3 % | |
Water absorption rate | Saturation,23°C | ISO 62 | 5.2to5.8 % |
impact performance | Test Condition | Test Method | AKRO-PLASTIC GERMANY/A3 GF 30 |
---|---|---|---|
Impact strength of simply supported beam without notch | -30°C | ISO 179/1eU | 80 kJ/m² |
23°C | ISO 179/1eU | 85 kJ/m² |
flammability | Test Condition | Test Method | AKRO-PLASTIC GERMANY/A3 GF 30 |
---|---|---|---|
Burning rate | 1.00mm | FMVSS302 | <100 mm/min |
UL flame retardant rating | 1.6mm | UL 94 | HB |