Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PVDC SARANEX™ 23P DOW USA
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
| film | Test Condition | Test Method | DOW USA/SARANEX™ 23P |
|---|---|---|---|
| consumption | 50.8μm | ASTM D4321 | 19.2 m²/kg |
| elongation | MD:Break,51μm | ASTM D882 | 370 % |
| TD:Break,51μm | ASTM D882 | 510 % | |
| film thickness | ASTM D374 | 51 µm | |
| 2.0mil(51µ | |||
| Heat sealing strength | TD | Internal Method | 540 N/m |
| MD | Internal Method | 540 N/m | |
| Oxygen permeability | 23°C,50%RH,51μm | ASTM D3985 | 12 cm³/m²/24hr |
| Secant modulus | 2%Secant,MD:51μm | ASTM D882 | 193 MPa |
| 2%Secant,TD:51μm | ASTM D882 | 221 MPa | |
| tensile strength | MD:Break,51μm | ASTM D882 | 24.1 MPa |
| TD:Break,51μm | ASTM D882 | 17.2 MPa | |
| Water vapor permeability | 38°C,90%RH,51μm | ASTMF1249 | 3.9 g/m²/24hr |