Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PC TA-35 MITSUBISHI RAYON AMERICA
--
Application in the automotive field
Good impact resistance, good weather resistance, and high heat resistance
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Mechanical properties | Test Condition | Test Method | MITSUBISHI RAYON AMERICA/TA-35 |
---|---|---|---|
tensile strength | 屈服 | ASTM D-638 | 44.1 MPa |
Rockwell hardness | ASTM D-785 | 100 R Scale | |
elongation at yield | ASTM D-638 | 80 % | |
Impact strength of cantilever beam gap | -40℃ | ASTM D-256 | 150 J/m |
bending strength | 屈服 | ASTM D-790 | 64.7 MPa |
Impact strength of cantilever beam gap | 23℃ | 600 | |
Flexural modulus | ASTM D-790 | 1860 MPa | |
Suspended wall beam without notch impact strength | 23℃ | 785 |
physical property | Test Condition | Test Method | MITSUBISHI RAYON AMERICA/TA-35 |
---|---|---|---|
Water absorption rate | 24hr | ASTM D-570 | 0.20 % |
density | ASTM D-792 | 1.15 g/cm3 | |
Shrinkage rate | MD | ASTM D-955 | 0.55 % |
Thermal performance | Test Condition | Test Method | MITSUBISHI RAYON AMERICA/TA-35 |
---|---|---|---|
UL flame retardant rating | 1.59mm | UL 94 | HB |
Linear coefficient of thermal expansion | 流动 | ASTM D-696 | 0.000085 cm/cm/℃ |
Heat distortion temperature | 0.45MPa,未退火,HDT | ASTM D-648 | 131 ℃ |
melting temperature | 230-270 ℃ | ||
Heat distortion temperature | 1.8MPa,未退火,HDT | 114 |