Material Comparison

Product Info
Product Name
Brand Name
Usages
Properties
Certificates
PA6 K225-KV DSM Additive Manufacturing
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--

Plastic Datasheets

Impact resistanceTest ConditionTest MethodDSM Additive Manufacturing/ K225-KV
Charpy Notched Impact Strength23°CISO 179/1eA4.0 kJ/m²
-30°CISO 179/1eA3.0 kJ/m²
Impact strength of simply supported beam without notch23°CISO 179/1eU40 kJ/m²
Mechanical propertiesTest ConditionTest MethodDSM Additive Manufacturing/ K225-KV
Nominal tensile fracture strainISO 527-24.0 %
Tensile modulusISO 527-24200 MPa
Tensile strain屈服ISO 527-23.0 %
tensile strength 屈服ISO 527-270.0 MPa
Electrical performanceTest ConditionTest MethodDSM Additive Manufacturing/ K225-KV
Compared to the Leakage Tracking Index (CTI)IEC 60112PLC 0
dielectric strengthIEC 60243-130 kV/mm
Volume resistivityIEC 60093>1.0E+15 ohms·cm
relative permittivity100HzIEC 602503.30
Dissipation Factor100HzIEC 602509E-03
relative permittivity1MHzIEC 602503.20
Surface ResistivityIEC 60093-- ohms
Dissipation Factor1MHzIEC 602500.020
flammabilityTest ConditionTest MethodDSM Additive Manufacturing/ K225-KV
Hot filament ignition temperature0.38mmIEC 60695-2-13930 °C
UL flame retardant rating3.0mmIEC 60695-11-10,-20V-2
Burning wire flammability index3.0mmIEC 60695-2-12960 °C
0.38mmIEC 60695-2-12960 °C
Hot filament ignition temperature3.0mmIEC 60695-2-13850 °C
UL flame retardant rating0.38mmIEC 60695-11-10,-20V-2
physical property Test ConditionTest MethodDSM Additive Manufacturing/ K225-KV
Shrinkage rateTDISO 294-41.0 %
MDISO 294-41.0 %
Water absorption rate平衡,23°C,50%RHISO 622.0 %
饱和,23°CISO 627.5 %
densityISO 11831.21 g/cm³
Thermal performanceTest ConditionTest MethodDSM Additive Manufacturing/ K225-KV
melting temperatureISO 11357-3220 °C