Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

EVA H2020 TPC SINGAPORE
COSMOTHENE®
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Thermal Properties | Test Condition | Test Method | TPC SINGAPORE/H2020 |
---|---|---|---|
Brittleness Temperature | ASTMD746 | <-75.0 °C | |
Vicat Softening Temperature | ASTMD1525 | 68.0 °C |
Hardness | Test Condition | Test Method | TPC SINGAPORE/H2020 |
---|---|---|---|
Shore Hardness | 邵氏D | ASTMD2240 | 30 |
Physical | Test Condition | Test Method | TPC SINGAPORE/H2020 |
---|---|---|---|
Environmental Stress Cracking Resistance | ASTMD1693 | >300 hr | |
Density / Specific Gravity | ASTMD792 | 0.930 g/cm³ | |
Melt Mass-Flow Rate | ASTMD1238 | 1.5 g/10min | |
Vinyl Acetate Content | 15.0 wt% |
Mechanical Properties | Test Condition | Test Method | TPC SINGAPORE/H2020 |
---|---|---|---|
Tensile Elongation | 断裂 | ASTMD638 | 800 % |
Flexural Modulus | ASTMD747 | 58.8 Mpa | |
Tensile Strength | 断裂 | ASTMD638 | 21.6 Mpa |