Material Comparison

Product Info
Product Name
Brand Name
Usages
Properties
Certificates
ABS GC-0700 BK Samsung Cheil South Korea
STAREX® 
Special material for bott、Automotive components
transparent、High temperature resistan
UL
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--

Plastic Datasheets

Impact resistanceTest ConditionTest MethodSamsung Cheil South Korea/GC-0700 BK
Suspended wall beam gap impact strength 523°CISO180/1A40 kJ/m²
Impact strength of cantilever beam gap23°C,6.35mmASTMD256200 J/m
23°C,3.18mmASTMD256390 J/m
hardnessTest ConditionTest MethodSamsung Cheil South Korea/GC-0700 BK
Rockwell hardnessR级ASTMD78595
R级ISO2039-295
Mechanical propertiesTest ConditionTest MethodSamsung Cheil South Korea/GC-0700 BK
Tensile stress断裂ISO527-2/5031.0 Mpa
屈服ISO527-2/5043.0 Mpa
elongation断裂ASTMD63817 %
Flexural modulusASTMD7901700 Mpa
tensile strength屈服ASTMD63843.0 Mpa
Bending stressISO17849.0 Mpa
tensile strength断裂ASTMD63826.0 Mpa
Tensile strain断裂ISO527-2/5011 %
Tensile modulusASTMD6381800 Mpa
Flexural modulusISO1781760 Mpa
Tensile modulusISO527-2/502000 Mpa
ASTMD79049.0 Mpa
flammabilityTest ConditionTest MethodSamsung Cheil South Korea/GC-0700 BK
UL flame retardant rating3.0mmUL94HB
physical property Test ConditionTest MethodSamsung Cheil South Korea/GC-0700 BK
Shrinkage rateMD:3.20mmASTMD9550.40to0.70 %
melt mass-flow rate250°C/10.0kgISO113340 g/10min
densityASTMD7921.09 g/cm³
melt mass-flow rate250°C/10.0kgASTMD123840 g/10min
densityISO11831.09 g/cm³
Thermal performanceTest ConditionTest MethodSamsung Cheil South Korea/GC-0700 BK
0.45MPa,Unannealed,4.00mmISO75-2/B85.0 °C
1.8MPa,Annealed,4.00mmISO75-2/A89.0 °C
1.8MPa,未退火,6.40mmASTMD64880.0 °C
0.45MPa,Annealed,4.00mmISO75-2/B97.0 °C
vicat--ISO306/B5090.0 °C
--ISO306/B12094.0 °C
0.45MPa,未退火,6.40mmASTMD64895.0 °C
1.8MPa,Unannealed,4.00mmISO75-2/A73.0 °C