Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PA6 6VOM DOMO CHEM GERMANY
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
| thermal performance | Test Condition | Test Method | DOMO CHEM GERMANY/6VOM |
|---|---|---|---|
| Hot deformation temperature | 0.45MPa,Unannealed | ISO 75-2/B | 180 °C |
| 1.8MPa,Unannealed | ISO 75-2/A | 70.0 °C | |
| Melting temperature | ISO 11357-3 | 218to222 °C | |
| Vicat softening temperature | ISO 306/B50 | 205 °C |
| mechanical properties | Test Condition | Test Method | DOMO CHEM GERMANY/6VOM |
|---|---|---|---|
| Bending modulus | ISO 178 | 3200 Mpa | |
| Tensile modulus | ISO 527-2/1 | 3400 Mpa | |
| Tensile strain | Break | ISO 527-2/50 | 15 % |
| Yield | ISO 527-2/50 | 8.0 % | |
| tensile strength | Yield | ISO 527-2/50 | 80.0 Mpa |
| Break | ISO 527-2/50 | 65.0 Mpa |
| Electrical performance | Test Condition | Test Method | DOMO CHEM GERMANY/6VOM |
|---|---|---|---|
| Compared to the anti leakage trace index | SolutionA | IEC 60112 | PLC 0 |
| Surface resistivity | IEC 60093 | 1E+13 ohms | |
| Volume resistivity | IEC 60093 | 1E+15 ohms·cm |
| Physical properties | Test Condition | Test Method | DOMO CHEM GERMANY/6VOM |
|---|---|---|---|
| density | ISO 1183 | 1.17 g/cm³ | |
| Water absorption rate | Saturation,23°C | ISO 62 | 9.0 % |
| impact performance | Test Condition | Test Method | DOMO CHEM GERMANY/6VOM |
|---|---|---|---|
| Charpy Notched Impact Strength | 23°C | ISO 179/1eA | 3.0 kJ/m² |
| Impact strength of cantilever beam gap | 23°C | ISO 180/1A | 3.0 kJ/m² |
| Impact strength of simply supported beam without notch | 23°C | ISO 179/1eU | 80 kJ/m² |
| flammability | Test Condition | Test Method | DOMO CHEM GERMANY/6VOM |
|---|---|---|---|
| Burning wire flammability index | 1.0to3.0mm | IEC 60695-2-12 | 960 °C |
| UL flame retardant rating | 0.8mm | UL 94 | V-0 |