Material Comparison

Product Info
Product Name
Brand Name
Usages
Properties
Certificates
PP TOLEN H085 CF SIBUR RUSSIA
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--

Plastic Datasheets

Impact resistanceTest ConditionTest MethodSIBUR RUSSIA/TOLEN H085 CF
Impact strength of cantilever beam gap23°CISO 1802.0 kJ/m²
Mechanical propertiesTest ConditionTest MethodSIBUR RUSSIA/TOLEN H085 CF
Flexural modulusISO 1781300 MPa
Tensile strain屈服ISO 527-2/5010 %
tensile strength 屈服ISO 527-2/5034.0 MPa
physical property Test ConditionTest MethodSIBUR RUSSIA/TOLEN H085 CF
melt mass-flow rate230°C/2.16kgISO 11338.5 g/10min
Thermal performanceTest ConditionTest MethodSIBUR RUSSIA/TOLEN H085 CF
Heat distortion temperature0.45MPa,未退火,HDTISO 75-2/B80.0 °C
vicatISO 306/A155 °C

Contact Us

Get App

Top