Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PBT LIHAN® T9706EP Nanjing Lihan Chemical Co., Ltd.
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Impact resistance | Test Condition | Test Method | Nanjing Lihan Chemical Co., Ltd./LIHAN® T9706EP |
---|---|---|---|
Impact strength of cantilever beam gap | ISO 180 | 10 kJ/m² |
hardness | Test Condition | Test Method | Nanjing Lihan Chemical Co., Ltd./LIHAN® T9706EP |
---|---|---|---|
Rockwell hardness | R计秤 | ISO 2039-2 | 119 |
Mechanical properties | Test Condition | Test Method | Nanjing Lihan Chemical Co., Ltd./LIHAN® T9706EP |
---|---|---|---|
tensile strength | 断裂 | ISO 527-2 | 125 MPa |
Tensile strain | 断裂 | ISO 527-2 | 2.1 % |
Flexural modulus | ISO 178 | 9000 MPa | |
bending strength | ISO 178 | 170 MPa |
Electrical performance | Test Condition | Test Method | Nanjing Lihan Chemical Co., Ltd./LIHAN® T9706EP |
---|---|---|---|
dielectric strength | ASTM D149 | 20 kV/mm | |
Surface Resistivity | ASTM D257 | 1E+13 ohms |
flammability | Test Condition | Test Method | Nanjing Lihan Chemical Co., Ltd./LIHAN® T9706EP |
---|---|---|---|
UL flame retardant rating | 1.6mm | UL 94 | V-0 |
physical property | Test Condition | Test Method | Nanjing Lihan Chemical Co., Ltd./LIHAN® T9706EP |
---|---|---|---|
Shrinkage rate | 0.30to1.0 % | ||
density | ISO 1183 | 1.68 g/cm³ | |
water content | ISO 62 | 0.40 % |
Thermal performance | Test Condition | Test Method | Nanjing Lihan Chemical Co., Ltd./LIHAN® T9706EP |
---|---|---|---|
Heat distortion temperature | 0.45MPa,未退火,HDT | ISO 75-2/B | 220 °C |
1.8MPa,未退火,HDT | ISO 75-2/A | 205 °C | |
Linear coefficient of thermal expansion | MD | ASTM D696 | 2.0E-5到3.0E-5 cm/cm/°C |
melting temperature | DSC | 220to225 °C |