Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

TPU 1195A10TR BASF JAPAN
Elastollan®
household electrical appl、Electrical applications、Automotive Applications、Cable
Hydrolysis resistance、Low temperature resistanc
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
hardness | Test Condition | Test Method | BASF JAPAN/1195A10TR |
---|---|---|---|
邵氏A | ASTMD2240 | 95 |
Mechanical properties | Test Condition | Test Method | BASF JAPAN/1195A10TR |
---|---|---|---|
Tensile modulus | 注塑 | ASTMD412 | 51.7 Mpa |
ASTMD1044 | 55.0 mg | ||
Abrasion-DIN | DIN53516 | 25 mm³ | |
Flexural modulus | 注塑 | ASTMD790 | 52.4 Mpa |
flammability | Test Condition | Test Method | BASF JAPAN/1195A10TR |
---|---|---|---|
UL flame retardant rating | 0.75mm | UL94 | HB |
3.0mm | UL94 | HB |
physical property | Test Condition | Test Method | BASF JAPAN/1195A10TR |
---|---|---|---|
melt mass-flow rate | 210°C/10.0kg | ASTMD1238 | 35to65 g/10min |
elastomer | Test Condition | Test Method | BASF JAPAN/1195A10TR |
---|---|---|---|
elongation | 断裂 | ASTMD412 | 430 % |
tensile strength | ASTMD412 | 39.3 Mpa | |
Tensile stress | 100%应变 | ASTMD412 | 17.2 Mpa |
Tear strength 2 | ASTMD624 | 140 kN/m | |
compression set | 23°C,22hr | ASTMD395B | 30 % |
Tensile stress | 300%应变 | ASTMD412 | 35.9 Mpa |
compression set | 70°C,22hr | ASTMD395B | 45 % |
Thermal performance | Test Condition | Test Method | BASF JAPAN/1195A10TR |
---|---|---|---|
Glass Transition Temperature | 内部方法 | -28.0 °C | |
SofteningPoint-DMA | 内部方法 | 89 °C | |
vicat | ASTMD1525 | 127 °C |