EAA 3004 STYRON US
PRIMACOR™
Electric wire,Cable
Heat sealing performance,High toughness,Resistance to stress crac
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Basic Performance | Test Condition | Test Method | STYRON US/3004 |
---|---|---|---|
melt mass-flow rate | 190℃/2.16kg | ASTM D-1238 | 8.5 g/10min |
190℃/2.16kg | ISO 1133 | 8.5 g/10min |
thermal performance | Test Condition | Test Method | STYRON US/3004 |
---|---|---|---|
Melting temperature | Internal Method | 98.0 °C | |
Vicat softening temperature | ASTMD1525 | 81.1 °C | |
ISO 306 | 81.1 ℃ | ||
ASTM D-1525 | 81.1 ℃ |
mechanical properties | Test Condition | Test Method | STYRON US/3004 |
---|---|---|---|
elongation | Break,Compression Molded | ASTMD638 | 600 % |
Elongation at Break | Compression Molded | ISO 527-2 | 600 % |
Compression Molded | ASTM D-638 | 600 % | |
tensile strength | Yield,Compression Molded | ISO 527-2 | 7.93 MPa |
Yield,Compression Molded | ASTM D-638 | 7.93 MPa | |
Compression Molded,Break | ISO 527-2 | 17.6 MPa | |
Break,Compression Molded | ASTMD638 | 17.6 Mpa | |
Yield,Compression Molded | ASTMD638 | 7.93 Mpa | |
Compression Molded,Break | ASTM D-638 | 17.6 MPa |
Physical properties | Test Condition | Test Method | STYRON US/3004 |
---|---|---|---|
Content of comonomer | 9.7 % | ||
density | ASTMD792 | 0.938 g/cm³ | |
ASTM D-792 | 0.938 g/cm³ | ||
ISO 1183 | 0.938 g/cm³ | ||
melt mass-flow rate | 190°C/2.16kg | ASTMD1238 | 8.5 g/10min |