Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PMMA EG-920 LX MMA KOREA
LGMMA®
Casters、Automotive sector、Electrical appliances
transparent、High rigidity
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Electrical performance | Test Condition | Test Method | LX MMA KOREA/EG-920 |
---|---|---|---|
dielectric constant | 60Hz | ASTM D-150 | 4 |
Loss factor | 60Hz | ASTM D-150 | 0.05 |
Volume resistivity | ASTM D-257 | >15 Ω.m | |
dielectric strength | 4KV/S | ASTM D-149 | 20 KV/mm |
Mechanical properties | Test Condition | Test Method | LX MMA KOREA/EG-920 |
---|---|---|---|
Rockwell hardness | ASTM D-785 | 93 M-scale | |
tensile strength | ASTM D-638 | 730 kg/cm | |
Impact strength of cantilever beam gap | Izod Notched | ASTM D-256 | 1.6 kg·cm/cm |
Flexural modulus | ASTM D-790 | 33.000 kg/cm | |
elongation at break | ASTM D-638 | 3.5 % | |
bending strength | ASTM D-790 | 1.300 kg/cm |
physical property | Test Condition | Test Method | LX MMA KOREA/EG-920 |
---|---|---|---|
transparency | 3.2mm | ASTM D-1003 | 93 % |
density | ASTM D-792 | 1.18 | |
Water absorption rate | 24h | ASTM D-570 | 0.3 % |
reflectivity | ASTM D-542 | 1.49 |
Thermal performance | Test Condition | Test Method | LX MMA KOREA/EG-920 |
---|---|---|---|
Heat distortion temperature | 18.56kg,HDT | ASTM D-648 | 96 °C |
Shrinkage rate | ASTM D995-51 | 0.2-0.6 % | |
melt mass-flow rate | 230°C,3.8kg | ASTM D-1238 | 1.6 g/10min |
Coefficient of sponge expansion | ASTM D-696 | 6×10 cm/cm/°C | |
specific heat | 0.35 cal/g/°C | ||
vicat | 1kg | ASTM D-1525 | 100 °C |
UL flame retardant rating | 1/8",1/16" | UL 94 | HB |
heat conduction | ASTM D-177 | 5×10 cal/seccm·°C/cm |
Contact Us
Get App
Top