| mechanical properties | Test Condition | Test Method | CELANESE USA/GUR 4022 |
|---|---|---|---|
| Tensile modulus | ISO 527-2/1A/1 | 3200 Mpa | |
| Charpy Notched Impact Strength | 23℃ | ISO 179/1eA | 3.5 kJ/m² |
| Tensile strain | Break | ISO 527-2/1A/5 | 8.0 % |
| bending strength | 23℃ | ISO 178 | 8600 Mpa |
| tensile strength | Break | ISO 527-2/1A/5 | 58 Mpa |
| Basic Performance | Test Condition | Test Method | CELANESE USA/GUR 4022 |
| density | ISO 1183 | 1.46 g/cm³ | |
| Shrinkage rate | Flow | ISO 294-4 | 1.8-2.0 % |
| thermal performance | Test Condition | Test Method | CELANESE USA/GUR 4022 |
| Hot deformation temperature | 1.8MPa,Unannealed | ISO 75-2/A | 63 °C |
| Other performance | Test Condition | Test Method | CELANESE USA/GUR 4022 |
| UL flame retardant rating | UL 94 | HB |