Material Comparison
Add Comparison Model
Highlight Differences
Hide Same

Product Name / Manufacturer / Model

Brand

Typical Applications

Properties

Color

Form

Processing Methods

Grade

Filler

Recycled Content

Certificates

Reference Price

elastomerTest ConditionTest MethodLCY TAIWAN/4075A NT
elongationBreak,23°CISO 37500 %
tensile strengthBreak,23°CISO 378.00 Mpa
tear strength23°CISO 34-123 kN/m
Permanent compression deformation70°C,22hrISO 81540 %
125°C,70hrISO 81564 %
tensile strength100%Strain,23°CISO 373.60 Mpa
thermal performanceTest ConditionTest MethodLCY TAIWAN/4075A NT
Melting temperatureInternal Method155 °C
Brittle temperatureISO 812-65.0 °C
hardnessTest ConditionTest MethodLCY TAIWAN/4075A NT
Shore hardnessShoreA,15Sec,InjectionISO 86878