Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

COC OKP-1 OSAKA GAS JAPAN
Polyester
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
| thermal performance | Test Condition | Test Method | OSAKA GAS JAPAN/OKP-1 |
|---|---|---|---|
| Glass transition temperature | 132 °C | ||
| Hot deformation temperature | 1.80MPa | 115 °C | |
| Linear coefficient of thermal expansion | 7.1 ×10-5/℃ |
| optical performance | Test Condition | Test Method | OSAKA GAS JAPAN/OKP-1 |
|---|---|---|---|
| birefringence | OGC法 | <5 ×10-4 | |
| Refractive index | D线 | 1.642 | |
| -12 ×10-5/℃ |