Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

TPE EM630 DSM HOLAND
Arnite®
--
Thermal stability
UL
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
hardness | Test Condition | Test Method | DSM HOLAND/EM630 |
---|---|---|---|
Shore hardness | Shore D, 3 Sec | ISO 868 | 60 |
thermal performance | Test Condition | Test Method | DSM HOLAND/EM630 |
---|---|---|---|
Linear coefficient of thermal expansion | Across Flow | ISO 11359-2 | 1.9E-4 cm/cm/°C |
Flow | ISO 11359-2 | 1.9E-4 cm/cm/°C | |
Melting temperature | ISO 11357-3 | 212 °C | |
Vicat softening temperature | ISO 306/B50 | 125 °C |
mechanical properties | Test Condition | Test Method | DSM HOLAND/EM630 |
---|---|---|---|
Nominal tensile fracture strain | ISO 527-2 | > 50 % | |
Tensile modulus | ISO 527-2 | 280 Mpa | |
Tensile strain | Yield | ISO 527-2 | 29 % |
Break | ISO 527-2 | > 300 % | |
tensile strength | 100% Strain | ISO 527-2 | 22.0 Mpa |
300% Strain | ISO 527-2 | 20.0 Mpa | |
5.0% Strain | ISO 527-2 | 12.5 Mpa | |
Yield | ISO 527-2 | 22.0 Mpa | |
50% Strain | ISO 527-2 | 21.0 Mpa | |
Break | ISO 527-2 | 31.5 Mpa | |
10% Strain | ISO 527-2 | 18.0 Mpa |
Electrical performance | Test Condition | Test Method | DSM HOLAND/EM630 |
---|---|---|---|
Compared to the anti leakage trace index | IEC 60112 | PLC 0 | |
Dielectric strength | IEC 60243-1 | 22 KV/mm | |
Dissipation factor | 100 Hz | IEC 60250 | 0.011 |
1 MHz | IEC 60250 | 0.034 | |
Relative permittivity | 100 Hz | IEC 60250 | 3.80 |
1 MHz | IEC 60250 | 3.40 | |
Volume resistivity | IEC 60093 | 1.0E+14 ohms·cm |
Physical properties | Test Condition | Test Method | DSM HOLAND/EM630 |
---|---|---|---|
Apparent density | ISO 60 | 0.76 g/cm³ | |
Melt Volume Flow Rate (MVR) | 230°C/2.16 kg | ISO 1133 | 4.00 cm3/10min |
Water absorption rate | Saturation, 23°C | ISO 62 | 0.60 % |
Equilibrium, 23°C, 50% RH | ISO 62 | 0.20 % |
flammability | Test Condition | Test Method | DSM HOLAND/EM630 |
---|---|---|---|
Flammability level | UL 94 | HB |
elastomer | Test Condition | Test Method | DSM HOLAND/EM630 |
---|---|---|---|
tear strength | ISO 34-1 | 180 kN/m |