Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

TPV 701-80 CELANESE USA
Santoprene™
Industrial applications,Automotive Applications,Application in the automotive field
Dimensional stability,Ozone resistant,Recyclable,Low tenderness,Oil resistant
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
hardness | Test Condition | Test Method | CELANESE USA/701-80 |
---|---|---|---|
Shore hardness | ShoreA,15Sec,23°C | ISO 868 | 83 |
thermal performance | Test Condition | Test Method | CELANESE USA/701-80 |
---|---|---|---|
Brittle temperature | ISO 812 | -32.0 °C | |
ASTM D746 | -32.0 °C |
elastomer | Test Condition | Test Method | CELANESE USA/701-80 |
---|---|---|---|
elongation | Break,23°C,Across Flow | ISO 37 | 290 % |
Break,23°C,Across Flow | ASTM D412 | 290 % | |
Permanent compression deformation | 70°C,22hr | ISO 815 | 30 % |
125°C,70hr | ISO 815 | 47 % | |
70°C,22hr | ASTM D395B | 30 % | |
125°C,70hr | ASTM D395B | 47 % | |
tear strength | 23°C,横向Flow | ASTM D624 | 30.0 kN/m |
23°C,Across Flow (Across Flow) | ISO 34-1 | 30 kN/m | |
tensile strength | Break,23°C | ISO 37 | 8.80 Mpa |
Break,23°C,横向Flow | ASTM D412 | 8.80 Mpa | |
Tensile stress | 100%Strain,23°C,横向Flow | ASTM D412 | 5.20 Mpa |
100%Strain,23°C,横向Flow | ISO 37 | 5.20 Mpa |
aging | Test Condition | Test Method | CELANESE USA/701-80 |
---|---|---|---|
Change rate of tensile strength in air | 125°C,70hr,inIRM903Oil | ASTM D471 | -38 % |
125°C,168hr | ISO 188 | 6.0 % | |
125°C,168hr | ASTM D573 | 6.0 % | |
Change rate of ultimate elongation in air | 125°C,70hr,inIRM903Oil | ISO 1817 | -48 % |
Elongation at Break | 125°C,70hr,inIRM903Oil | ASTM D471 | -48 % |
125°C,168hr | ASTM D573 | -37 % | |
Hardness change rate in the air | ShoreA,125°C,168hr | ASTM D573 | 2.0 |
Shore hardness | ShoreA,125°C,168hr | ISO 188 | 2.0 |
Tensile strain change rate | 125°C,70hr,inIRM903Oil | ISO 1817 | -38 % |
Volume change | 125°C,70hr,在IRM903油中 | ISO 1817 | 4.0 % |