PA66 Staramide RF00ASXP EUROSTAR FRANCE
--
--
Filler, glass fiber reinforced material, 50%, filler by weight
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Impact resistance | Test Condition | Test Method | EUROSTAR FRANCE/Staramide RF00ASXP |
---|---|---|---|
Suspended wall beam without notch impact strength | 23°C | ISO 180/1U | 80 kJ/m² |
Impact strength of cantilever beam gap | 23°C | ISO 180/1A | 15 kJ/m² |
Electrical performance | Test Condition | Test Method | EUROSTAR FRANCE/Staramide RF00ASXP |
---|---|---|---|
High arc combustion index (HAI) | HAI | UL 746 | PLC 0 |
Hot wire ignition (HWI) | HWI | UL 746 | PLC 4 |
Mechanical properties | Test Condition | Test Method | EUROSTAR FRANCE/Staramide RF00ASXP |
---|---|---|---|
tensile strength | 屈服 | ISO 527-2/5 | 210 MPa |
Tensile strain | 断裂 | ISO 527-2/5 | 2.4 % |
Flexural modulus | ISO 178 | 14100 MPa | |
Tensile modulus | ISO 527-2/1 | 15400 MPa | |
bending strength | ISO 178 | 305 MPa |
flammability | Test Condition | Test Method | EUROSTAR FRANCE/Staramide RF00ASXP |
---|---|---|---|
UL flame retardant rating | 1.5mm | UL 94 | HB |
physical property | Test Condition | Test Method | EUROSTAR FRANCE/Staramide RF00ASXP |
---|---|---|---|
Shrinkage rate | MD:4.00mm | 内部方法 | 0.10to0.30 % |
Water absorption rate | 23°C,24hr | ISO 62 | 0.70 % |
density | ISO 1183 | 1.57 g/cm³ |
Thermal performance | Test Condition | Test Method | EUROSTAR FRANCE/Staramide RF00ASXP |
---|---|---|---|
Heat distortion temperature | 0.45MPa,未退火,64.0mm跨距,HDT | ISO 75-2/Bf | 259 °C |
Linear coefficient of thermal expansion | TD:23到60°C | ISO 11359-2 | 8.4E-05 cm/cm/°C |
MD:23到60°C | ISO 11359-2 | 2.6E-05 cm/cm/°C | |
RTI Imp | UL 746 | 125 °C | |
Heat distortion temperature | 1.8MPa,未退火,64.0mm跨距,HDT | ISO 75-2/Af | 246 °C |
RTI | UL 746 | 125 °C | |
RTI Elec | UL 746 | 130 °C |