Plastic Datasheets

Impact resistanceTest ConditionTest MethodSoredi S.p.a./Nirion F30
Impact strength of cantilever beam gap-20°C,3.20mmASTM D25680 J/m
23°C,3.20mmASTM D256150 J/m
hardnessTest ConditionTest MethodSoredi S.p.a./Nirion F30
Rockwell hardnessR级ASTM D78585
Electrical performanceTest ConditionTest MethodSoredi S.p.a./Nirion F30
Volume resistivityIEC 600931E+14 ohms·cm
dielectric strength1.00mmIEC 60243-130 kV/mm
relative permittivity1MHzIEC 602503.20
Surface ResistivityIEC 600931E+15 ohms
Dissipation Factor1MHzIEC 602509E-03
Mechanical propertiesTest ConditionTest MethodSoredi S.p.a./Nirion F30
elongation断裂ASTM D6383.0 %
tensile strength 断裂ASTM D638110 MPa
Flexural modulusASTM D7908000 MPa
bending strength断裂ASTM D790160 MPa
flammabilityTest ConditionTest MethodSoredi S.p.a./Nirion F30
Hot filament ignition temperatureIEC 60695-2-13850 °C
UL flame retardant rating3.2mmUL 94V-1
1.6mmUL 94V-1
physical property Test ConditionTest MethodSoredi S.p.a./Nirion F30
Shrinkage rateMDASTM D9550.20to0.30 %
Water absorption rate平衡,23°C,50%RHISO 620.10 %
饱和,23°CISO 620.25 %
densityASTM D7921.44 g/cm³
melt mass-flow rate300°C/1.2kgASTM D12388.0 g/10min
Thermal performanceTest ConditionTest MethodSoredi S.p.a./Nirion F30
Heat distortion temperature1.8MPa,未退火,HDTASTM D648150 °C
vicatASTM D15254148 °C
Linear coefficient of thermal expansionMD:23到55°CISO 11359-22.5E-05 cm/cm/°C