Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PPS+PPE XYRON™ DG235 ASAHI JAPAN
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Impact resistance | Test Condition | Test Method | ASAHI JAPAN/XYRON™ DG235 |
---|---|---|---|
Charpy Notched Impact Strength | 23°C | ISO 179 | 7.0 kJ/m² |
Mechanical properties | Test Condition | Test Method | ASAHI JAPAN/XYRON™ DG235 |
---|---|---|---|
Flexural modulus | 23°C | ISO 178 | 9750 MPa |
Tensile strain | 断裂,23°C | ISO 527-2 | 2.0 % |
tensile strength | 屈服,23°C | ISO 527-2 | 125 MPa |
bending strength | 23°C | ISO 178 | 192 MPa |
Electrical performance | Test Condition | Test Method | ASAHI JAPAN/XYRON™ DG235 |
---|---|---|---|
dielectric constant | 100Hz | IEC 60250 | 4.00 |
Dissipation Factor | 100Hz | IEC 60250 | 1E-03 |
Volume resistivity | 23°C | IEC 60093 | 1E+16 ohms·cm |
dielectric constant | 1MHz | IEC 60250 | 4.00 |
Surface Resistivity | IEC 60093 | 1E+16 ohms | |
Dissipation Factor | 1MHz | IEC 60250 | 2E-03 |
flammability | Test Condition | Test Method | ASAHI JAPAN/XYRON™ DG235 |
---|---|---|---|
UL flame retardant rating | 0.75mm | UL 94 | V-1 |
physical property | Test Condition | Test Method | ASAHI JAPAN/XYRON™ DG235 |
---|---|---|---|
Shrinkage rate | 2.00mm | 内部方法 | 0.20to0.50 % |
density | ISO 1183 | 1.44 g/cm³ |
Thermal performance | Test Condition | Test Method | ASAHI JAPAN/XYRON™ DG235 |
---|---|---|---|
Linear coefficient of thermal expansion | MD:-30到65°C | ISO 11359-2 | 3.5E-05 cm/cm/°C |
Heat distortion temperature | 1.8MPa,未退火,HDT | ISO 75-2/A | 240 °C |