Material Comparison
Add Comparison Model
Select Products for Comparison (1/4)
Highlight Differences
Hide Same
Product Name / Manufacturer / Model
Grade
Certificates
Reference Price
| mechanical properties | Test Condition | Test Method | DUPONT USA/S650FR BK851 |
|---|---|---|---|
| bending strength | ISO 178 | 100 Mpa | |
| Tensile modulus | ISO 527-2 | 3000 Mpa | |
| Tensile strain | Yield | ISO 527-2 | 4.6 % |
| bending strength | ASTM D790/ISO 178 | 100 kg/cm²(MPa)[Lb/in²] | |
| Tensile modulus | ASTM D638/ISO 527 | 3000 kg/cm²(MPa)[Lb/in²] | |
| Nominal tensile fracture strain | ISO 527-2 | 7.2 % | |
| tensile strength | Yield | ISO 527-2 | 65.0 Mpa |
| flammability | Test Condition | Test Method | DUPONT USA/S650FR BK851 |
| UL flame retardant rating | 1.5mm | IEC 60695-11-10,-20 | V-0 |
| 0.75mm | UL 94 | V-0 | |
| Extreme Oxygen Index | ISO 4589-2 | 30 % | |
| UL flame retardant rating | 1.5mm | UL 94 | V-0 |
| FMVSS flammability | FMVSS302 | DNI | |
| UL flame retardant rating | 0.75mm | IEC 60695-11-10,-20 | V-0 |
| other | Test Condition | Test Method | DUPONT USA/S650FR BK851 |
| characteristic | 阻燃 | ||
| Physical properties | Test Condition | Test Method | DUPONT USA/S650FR BK851 |
| Shrinkage rate | MD | ISO 294-4 | 1.8 % |
| Top out temperature | 170 °C | ||
| Shrinkage rate | TD | ISO 294-4 | 1.6 % |
| density | ASTM D792/ISO 1183 | 1.46 | |
| Electrical performance | Test Condition | Test Method | DUPONT USA/S650FR BK851 |
| Dissipation factor | 100Hz | IEC 60250 | 7.4E-04 |
| Volume resistivity | IEC 60093 | >1.0E+15 ohms·cm | |
| Dissipation factor | 1MHz | IEC 60250 | 0.017 |
| Relative permittivity | 100Hz | IEC 60250 | 3.70 |
| Surface resistivity | IEC 60093 | 1E+13 ohms | |
| Relative permittivity | 1MHz | IEC 60250 | 3.50 |
| Dielectric strength | IEC 60243-1 | 33 KV/mm | |
| impact performance | Test Condition | Test Method | DUPONT USA/S650FR BK851 |
| Impact strength of simply supported beam without notch | 23°C | ISO 179/1eU | 60 kJ/m² |
| -30°C | ISO 179/1eU | 55 kJ/m² | |
| thermal performance | Test Condition | Test Method | DUPONT USA/S650FR BK851 |
| Hot deformation temperature | 0.45MPa,Unannealed | ISO 75-2/B | 160 °C |
| Combustibility (rate) | UL 94 | V-0 | |
| Hot deformation temperature | 1.8MPa,Unannealed | ISO 75-2/A | 65.0 °C |
| Melting temperature | ISO 11357-3 | 225 °C |