Material Comparison
Add Comparison Model
Select Products for Comparison (1/4)
Highlight Differences
Hide Same
Product Name / Manufacturer / Model
Reference Price
| film | Test Condition | Test Method | EXXONMOBIL SINGAPORE/1002XBU |
|---|---|---|---|
| Dart impact | 70 | ||
| Secant modulus | 1% Secant,TD | ASTM D882 | 220 Mpa |
| Elmendorf tear strength | MDMD | 90 g | |
| tensile strength | MD,YieldMD : Yield | 9.4 Mpa | |
| MD,BreakMD : Break | 49 Mpa | ||
| Tensile strain | TD,BreakTD : Break | 800 % | |
| Elmendorf tear strength | TDTD | 400 g | |
| tensile strength | TD,BreakTD : Break | 29 Mpa | |
| TD,YieldTD : Yield | 8.9 Mpa | ||
| Tensile strain | MD,BreakMD : Break | 590 % | |
| optical performance | Test Condition | Test Method | EXXONMOBIL SINGAPORE/1002XBU |
| turbidity | ASTM D1003 | 4.4 % | |
| gloss | 45°45° | ASTM D2457 | 76 |
| Physical properties | Test Condition | Test Method | EXXONMOBIL SINGAPORE/1002XBU |
| density | ASTM D1505 | 0.918 g/cm³ | |
| melt mass-flow rate | 190℃,2.16kg | ASTM D1238 | 2 g/10min |