LLDPE 1002XBU EXXONMOBIL SINGAPORE
ExxonMobil™
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Thin film | Test Condition | Test Method | EXXONMOBIL SINGAPORE/1002XBU |
---|---|---|---|
Tensile strength | TD,屈服 TD : Yield | 8.9 Mpa | |
70 | |||
Tensile strength | TD,断裂 TD : Break | 29 Mpa | |
Tensile strain | MD,断裂 MD : Break | 590 % | |
Elmondov tear strength | TD TD | 400 g | |
Secant modulus | 1% 正割,TD | ASTM D882 | 220 Mpa |
Elmondov tear strength | MD MD | 90 g | |
Tensile strength | MD,屈服 MD : Yield | 9.4 Mpa | |
MD,断裂 MD : Break | 49 Mpa | ||
Tensile strain | TD,断裂 TD : Break | 800 % |
Optical performance | Test Condition | Test Method | EXXONMOBIL SINGAPORE/1002XBU |
---|---|---|---|
Glossiness | 45° 45° | ASTM D2457 | 76 |
Haze ratio | ASTM D1003 | 4.4 % |
Physical performance | Test Condition | Test Method | EXXONMOBIL SINGAPORE/1002XBU |
---|---|---|---|
Melt mass flow rate | 190℃,2.16kg | ASTM D1238 | 2 g/10min |
Density | ASTM D1505 | 0.918 g/cm³ |