Material Comparison
Add Comparison Model
Select Products for Comparison (1/4)
Highlight Differences
Hide Same
Product Name / Manufacturer / Model
Grade
Reference Price
| thermal performance | Test Condition | Test Method | Korea Daelim Basell/EP310D |
|---|---|---|---|
| Hot deformation temperature | 0.45MPa Unannealed | ISO 75B-1 | 72 °C |
| Vicat softening temperature | A50(50℃/h 10N) | ISO 306 | 150 °C |
| Basic Performance | Test Condition | Test Method | Korea Daelim Basell/EP310D |
| density | ISO 1183 | 0.9 | |
| melt mass-flow rate | 230℃,2.16kg | ISO 1133 | 0.8 g/10min |
| mechanical properties | Test Condition | Test Method | Korea Daelim Basell/EP310D |
| Charpy Notched Impact Strength | 23℃,Type 1,Edgewise,Notch A | ISO 179 | 44 KJ/m |
| elongation at yield | 50mm/min | ISO 527-1 | 11 % |
| Elongation at Break | 50mm/min | ISO 527-1 | 420 % |
| Charpy Notched Impact Strength | 0℃,Type 1,Edgewise,Notch A | ISO 179 | 6 KJ/m |
| -20℃,Type 1,Edgewise,Notch A | ISO 179 | 4.2 KJ/m | |
| tensile strength | 50mm/min,Yield | ISO 527-1 | 27 Mpa |
| Bending modulus | ISO 527-1 | 1200 Mpa |