Copolyester GS4 Eastman Chemical Company
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--

Plastic Datasheets

Electrical performanceTest ConditionTest MethodEastman Chemical Company/ GS4
dielectric constant23°C,1kHzASTM D1503.20
23°C,1MHzASTM D1502.95
Surface ResistivityASTM D2572E+16 ohms
Dissipation Factor23°C,1kHzASTM D1500.017
Volume resistivity23°CASTM D2574.6E+16 ohms·cm
Dissipation Factor23°C,1MHzASTM D1500.022
dielectric strength23°CASTM D14916 kV/mm
arc resistanceASTM D495134 sec
flammabilityTest ConditionTest MethodEastman Chemical Company/ GS4
Limiting Oxygen IndexASTM D286325 %
physical property Test ConditionTest MethodEastman Chemical Company/ GS4
densityASTM D15051.28 g/cm³
Water absorption rate23°C,24hrASTM D5700.15 %
Thermal performanceTest ConditionTest MethodEastman Chemical Company/ GS4
Heat distortion temperature1.8MPa,未退火,HDTASTM D64863.0 °C
vicatASTM D152579.0 °C
specific heat60°CDSC1300 J/kg/°C
Glass Transition TemperatureDSC80.0 °C
Heat distortion temperature0.45MPa,未退火,HDTASTM D64868.0 °C
specific heat150°CDSC1800 J/kg/°C
200°CDSC2000 J/kg/°C
100°CDSC1700 J/kg/°C
250°CDSC2100 J/kg/°C
Linear coefficient of thermal expansionMD:23°CASTM D6967.6E-05 cm/cm/°C