PC 9925A-NA1A0036 SABIC INNOVATIVE US
LEXAN™
Electronic and electrical components,Thin walled products,Automotive sector
UV resistance,Thermal stability
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
thermal performance | Test Condition | Test Method | SABIC INNOVATIVE US/9925A-NA1A0036 |
---|---|---|---|
0.45MPa, unannealed, 64.0mm span | ISO 75-2/Bf | 135 °C | |
1.8MPa, unannealed, 3.20mm | ASTM D648 | 124 °C | |
1.8MPa, unannealed, 64.0mm span of | ISO 75-2/Af | 123 °C | |
Linear coefficient of thermal expansion | MD:-40to40°C | ASTME831 | 7E-05 cm/cm/°C |
TD:-40to40°C | ASTME831 | 7E-05 cm/cm/°C | |
Vicat softening temperature | ASTM D152513 | 140 °C |
mechanical properties | Test Condition | Test Method | SABIC INNOVATIVE US/9925A-NA1A0036 |
---|---|---|---|
--1 | ASTM D638 | 2300 Mpa | |
50.0mm span | ASTM D790 | 2150 Mpa | |
--7 | ISO 178 | 2240 Mpa | |
--8 | ISO 178 | 95.0 Mpa | |
crack | ISO 527-2/50 | 77 % | |
ASTM D638 | 60.0 Mpa | ||
ASTM D638 | 83 % | ||
ISO 527-2/50 | 56.0 Mpa | ||
yield | ASTM D638 | 6.0 % | |
ASTM D638 | 60.0 Mpa | ||
ISO 527-2/50 | 6.0 % | ||
ISO 527-2/50 | 62.0 Mpa | ||
Yield, 50.0mm span | ASTM D790 | 91.0 Mpa |
Physical properties | Test Condition | Test Method | SABIC INNOVATIVE US/9925A-NA1A0036 |
---|---|---|---|
melt mass-flow rate | 300°C/1.2kg | ASTM D1238 | 13 g/10min |
Shrinkage rate | MD:3.20mm | Internal Method | 0.50-0.70 % |
Water absorption rate | Equilibrium,23°C,50%RH | ISO 62 | 0.15 % |
Saturation,23°C | ISO 62 | 0.35 % |
impact performance | Test Condition | Test Method | SABIC INNOVATIVE US/9925A-NA1A0036 |
---|---|---|---|
Charpy Notched Impact Strength | 23°C | ISO 179/1eA | 68 kJ/m² |
Dart impact | 23°C,TotalEnergy | ASTM D3763 | 75.0 J |
flammability | Test Condition | Test Method | SABIC INNOVATIVE US/9925A-NA1A0036 |
---|---|---|---|
UL flame retardant rating | 1.50mm | UL 94 | V-0 |