Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

MDPE BPD4038 Malaysia ETILINAS
--
Communication and power cable sheath
Environmental stress cracking resistance, wear resistance, weather resistance, and thermal stability
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Other performance | Test Condition | Test Method | Malaysia ETILINAS/BPD4038 |
---|---|---|---|
Oxidation induction time (OIT) | 210℃ | ISO TR10837 | >20 min |
Basic performance | Test Condition | Test Method | Malaysia ETILINAS/BPD4038 |
---|---|---|---|
Carbon black content | IEC 811-4-1 | 2.5 % | |
melt mass-flow rate | 190℃/2.16kg | ISO 1133: Condition 4 | 0.3 g/10min |
190℃/5.0kg | ISO 1133: Condition 18 | 1.3 g/10min | |
density | ISO 1183 | 937 kg/m | |
Compound | ISO 1183 | 948 kg/m |
Mechanical properties | Test Condition | Test Method | Malaysia ETILINAS/BPD4038 |
---|---|---|---|
Shore hardness | ISO 868 (1 sec) | 58 | |
Flexural modulus | ISO 178 | 750 MPa | |
elongation | 断裂 | IEC 811-1-1 | >600 % |
Environmental stress cracking resistance | F0 | ASTM D-1693B | >1000 Hours |
Tensile stress | IEC 811-1-1 | 19 MPa |
Electrical performance | Test Condition | Test Method | Malaysia ETILINAS/BPD4038 |
---|---|---|---|
Volume resistivity | IEC 93 | >10 Ω.cm | |
dielectric constant | 1 MHz | IEC 250 | 2.5 |
Dissipation Factor | 1 MHz | IEC 250 | <0.001 |
dielectric strength | IEC 243 | 20 kV/mm |
Thermal performance | Test Condition | Test Method | Malaysia ETILINAS/BPD4038 |
---|---|---|---|
vicat | ISO 306 A | 116 ℃ | |
thermal conductivity | W/m℃ | BS 874(at 23℃) 0.4 | |
brittle temperature | ASTM D-746 | <-100 ℃ | |
Linear coefficient of thermal expansion | ASTM D-696(20-60℃) | 1.5 ℃ |
Contact Us