| flammability | Test Condition | Test Method | Samsung Cheil South Korea/CF-3300LW |
|---|---|---|---|
| UL flame retardant rating | 0.8mm | UL 94 | V-2 |
| 3.2mm | UL 94 | V-1 | |
| mechanical properties | Test Condition | Test Method | Samsung Cheil South Korea/CF-3300LW |
| elongation | Break | ASTM D638 | 3.8 % |
| bending strength | ISO 178 | 180 Mpa | |
| Tensile modulus | ISO 527-2/50 | 6900 Mpa | |
| bending strength | ASTM D790 | 170 Mpa | |
| Tensile modulus | ASTM D638 | 6400 Mpa | |
| tensile strength | Break | ISO 527-2/50 | 125 Mpa |
| Yield | ISO 527-2/50 | 125 Mpa | |
| Tensile strain | Break | ISO 527-2/50 | 3.8 % |
| tensile strength | Break | ASTM D638 | 120 Mpa |
| Yield | ASTM D638 | 120 Mpa | |
| Bending modulus | ASTM D790 | 6500 Mpa | |
| ISO 178 | 7300 Mpa | ||
| thermal performance | Test Condition | Test Method | Samsung Cheil South Korea/CF-3300LW |
| Vicat softening temperature | -- | ISO 306/B50 | 147 °C |
| Hot deformation temperature | 1.8MPa,Unannealed,6.40mm | ASTM D648 | 140 °C |
| 0.45MPa,Unannealed,4.00mm | ISO 75-2/B | 143 °C | |
| 0.45MPa,Unannealed,6.40mm | ASTM D648 | 143 °C | |
| Vicat softening temperature | -- | ISO 306/B120 | 148 °C |
| Hot deformation temperature | 1.8MPa,Unannealed,4.00mm | ISO 75-2/A | 138 °C |
| impact performance | Test Condition | Test Method | Samsung Cheil South Korea/CF-3300LW |
| Impact strength of cantilever beam gap | 23°C,3.18mm | ASTM D256 | 180 J/m |
| 23°C,6.35mm | ASTM D256 | 150 J/m | |
| 23°C | ISO 180/1A | 17 kJ/m² | |
| Charpy Notched Impact Strength | 23°C | ISO 179/1eA | 18 kJ/m² |
| Physical properties | Test Condition | Test Method | Samsung Cheil South Korea/CF-3300LW |
| density | ISO 1183 | 1.40 g/cm³ | |
| melt mass-flow rate | 250°C/10.0kg | ISO 1133 | 22 g/10min |
| Shrinkage rate | TD:3.20mm | ISO 2577 | 0.10-0.30 % |
| melt mass-flow rate | 250°C/10.0kg | ASTM D1238 | 22 g/10min |
| Shrinkage rate | MD:3.20mm | ASTM D955 | 0.10-0.30 % |
| density | ASTM D792 | 1.40 g/cm³ | |
| Shrinkage rate | MD:3.20mm | ISO 2577 | 0.10-0.30 % |
| TD:3.20mm | ASTM D955 | 0.10-0.30 % | |
| hardness | Test Condition | Test Method | Samsung Cheil South Korea/CF-3300LW |
| Rockwell hardness | R-Scale | ASTM D785 | 115 |
| R-Scale | ISO 2039-2 | 115 |