| flammability | Test Condition | Test Method | ASAHI JAPAN/HC460 V326200 |
|---|---|---|---|
| UL flame retardant rating | 0.75mm | UL 94 | HB |
| Physical properties | Test Condition | Test Method | ASAHI JAPAN/HC460 V326200 |
| Shrinkage rate | MD | Internal Method | 1.6-2.0 % |
| melt mass-flow rate | 190°C/2.16kg | ISO 1133 | 8.0 g/10min |
| Water absorption rate | 23°C,24hr,50%RH | ASTM D570 | 0.20 % |
| thermal performance | Test Condition | Test Method | ASAHI JAPAN/HC460 V326200 |
| Hot deformation temperature | 0.45MPa,Unannealed | ISO 75-2/B | 158 °C |
| specific heat | 1470 J/kg/°C | ||
| Hot deformation temperature | 1.8MPa,Unannealed | ASTM D648 | 124 °C |
| thermal conductivity | 0.23 W/m/K | ||
| Linear coefficient of thermal expansion | MD | ASTMD696 | 1E-04 cm/cm/°C |
| Hot deformation temperature | 0.45MPa,Unannealed | ASTM D648 | 163 °C |
| 1.8MPa,Unannealed | ISO 75-2/A | 102 °C | |
| mechanical properties | Test Condition | Test Method | ASAHI JAPAN/HC460 V326200 |
| Bending modulus | ASTMD790 | 2600 Mpa | |
| tensile strength | Yield | ISO 527-2 | 66.0 Mpa |
| Tensile modulus | ISO 527-2 | 2750 Mpa | |
| elongation | Break | ASTMD638 | 40 % |
| bending strength | ASTM D790 | 88.0 Mpa | |
| tensile strength | -- | ASTM D638 | 64.0 Mpa |
| hardness | Test Condition | Test Method | ASAHI JAPAN/HC460 V326200 |
| Rockwell hardness | M-Scale | ASTM D785 | 88 |
| R-Scale | ASTM D785 | 117 |