Material Comparison

Product Info
Product Name
Brand Name
Usages
Properties
Certificates
ABS VN30 BK ASAHI JAPAN
XYRON™
--
--
UL
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--

Plastic Datasheets

Impact resistanceTest ConditionTest MethodASAHI JAPAN/VN30 BK
Charpy Notched Impact Strength23°CISO 1796.0 kJ/m²
Electrical performanceTest ConditionTest MethodASAHI JAPAN/VN30 BK
Volume resistivity23°CIEC 600931E+16 ohms·cm
Surface ResistivityIEC 600931E+16 ohms
Mechanical propertiesTest ConditionTest MethodASAHI JAPAN/VN30 BK
bending strength23°CISO 17878.0 Mpa
tensile strength 屈服,23°CISO 527-246.0 Mpa
Flexural modulus23°CISO 1782000 Mpa
Nominal tensile fracture strain23°CISO 527-230 %
flammabilityTest ConditionTest MethodASAHI JAPAN/VN30 BK
UL flame retardant rating1.50mmUL 94V-1
physical property Test ConditionTest MethodASAHI JAPAN/VN30 BK
Shrinkage rate2.00mm内部方法0.50-0.70 %
Water absorption rate23°C,24hrISO 620.060 %
Thermal performanceTest ConditionTest MethodASAHI JAPAN/VN30 BK
1.8MPa, Not annealedASTM D648100 °C
Linear coefficient of thermal expansionMD:-30到65°CISO 11359-27.5E-05 cm/cm/°C
1.8MPa, Not annealedISO 75-2/A96.0 °C